Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 142 MPa | 20600 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Hardness, H358/30 | 142 MPa | 20600 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Hardness, H358/30 | 142 MPa | 20600 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |