Polymer Property : 50% Modulus = 1.42 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
50% Modulus 0.00980 GPa
1.42 ksi
ASMT D638
Toyobo Pelprene™ P-150M Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..
50% Modulus 0.00980 GPa
1.42 ksi
ASTM D638
Toyobo PELPRENE™ P55B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
50% Modulus 0.00980 GPa
1.42 ksi
ASTM D638
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
50% Modulus 0.00980 GPa
1.42 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR4525 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..