50% Modulus 0.000220 GPa
0.0319 ksi
UBE UBEPOL BR150 Synthetic Rubber (Compound)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
50% Modulus 0.000220 GPa
0.0319 ksi
UBE UBEPOL BR150B Synthetic Rubber (Compound)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
50% Modulus 0.000220 GPa
0.0319 ksi
UBE UBEPOL BR150L Synthetic Rubber (Compound)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
50% Modulus 0.000220 GPa
0.0319 ksi
ASTM D412
3M RJS--1 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
50% Modulus 0.000220 GPa
0.0319 ksi
ASTM D412
3M RJS-2 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
50% Modulus 0.000220 GPa
0.0319 ksi
ASTM D412
3M RJS-3 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
50% Modulus 0.000220 GPa
0.0319 ksi
ASTM D412
3M RJS-4 3/C Phase Rejacketing System
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of..
50% Modulus 0.000220 GPa
0.0319 ksi
ASTM D412
3M RJS-5 3/C Phase Rejacketing System