Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 4100 MPa

@Temperature 23.0 °C
595000 psi

@Temperature 73.4 °F
50%RH; ISO 899
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Creep Modulus, 1000 hours 4100 MPa
595000 psi
ISO 899-1
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber
30% Glass fiber reinforced; injection molding grade
Tensile Creep Modulus, 1000 hours 4100 MPa
595000 psi
ISO 899-1
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Tensile Creep Modulus, 1000 hours 4100 MPa
595000 psi
ISO 899-1
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
Tensile Creep Modulus, 1000 hours 4100 MPa
595000 psi
ISO 899-1
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber
PA 6, Injection molding grade, 30% glass fibers, weather stabilized