Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 4500 MPa | 653000 psi | ISO 899-1 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 4500 MPa | 653000 psi | ISO 899-1 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 4500 MPa | 653000 psi | ISO 899-1 |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 4500 MPa | 653000 psi | ISO 899-1 |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Tensile Creep Modulus, 1000 hours | 4500 - 12000 MPa | 653000 - 1.74e+6 psi | Average value: 7400 MPa Grade Count:10 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Creep Modulus, 1000 hours | 4500 MPa @Strain <=0.500 % |
653000 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |