Mechanical Properties Metric English Comments
Tenacity 2.03 - 2.38 N/tex
23.0 - 27.0 g/denier
Kuraray Vectran® HT 1500/300 LCP Fiber
 is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an..
Tenacity 2.03 N/tex
23.0 g/denier
Tensile Modulus
UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=5)
Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE.
Tenacity 2.03 N/tex
23.0 g/denier
DuPont™ Kevlar® 29 Aramid Fiber
1500 Denier; 1000 Filaments. Kevlar® 29 yarns are used in ballistic applications, ropes and cables, protective apparel such as cut-resistant gloves, in life protection uses such as helmets, vehicu..