Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | Sealing Initial Temperature; Braskem® Method |
Braskem PB 525/64 LDPE Blown Film Extrusion Polyethylene
(discontinued **) 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Automatic packaging of liquids products (FFS). Information provided by Braskem |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD11 is a general, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD12 is a printing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has co.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS12 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS12 is a printing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has coron.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 18 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 20 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 - 110 °C | 221 - 230 °F | Kinlead |
Kinlead LSS13 Low Temperature Grade Heat Sealable Film (thickness: 30 µm) LSS13 is a metalizing, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One side .. |
|||
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | |
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.Benefits. LX5 02-15 produc.. |
|||
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | 1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method |
Dow 4010 Low Density Polyethylene (LDPE) Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc.. |
|||
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | 1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method |
Dow 4012 Low Density Polyethylene (LDPE) Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow |
|||
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | 1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method |
Dow 722 Low Density Polyethylene (LDPE) Polyethylene 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist foods pac.. |
|||
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | Sealing Initial Temperature; Braskem® Method |
Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi.. |
|||
Heat Seal Strength Initiation Temperature | 105 °C | 221 °F | Sealing Initial Temperature; Braskem® Method |
Braskem EB 853/72 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose; automatic packaging of solids products (FFS). Informatio.. |
|||
Heat Seal Strength Initiation Temperature | 105 - 130 °C | 221 - 266 °F | Average value: 113 °C Grade Count:56 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |