Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.260 GPa | 37.7 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.260 GPa | 37.7 ksi | ASTM D882 |
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Secant Modulus, TD | 0.260 GPa | 37.7 ksi | ASTM D882-A |
Borealis Himod™ FT7293 LDPE for Film Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Secant Modulus, TD | 0.260 GPa | 37.7 ksi | ASTM D882-A |
Borealis Himod™ FT7294 LDPE for Film Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |