Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.703 GPa | 102 ksi | ASTM D 882 A |
Total Finathene® 6450 HDPE film
(discontinued **) Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin.. |
|||
Secant Modulus, TD | 0.700 GPa | 102 ksi | 0.05-1.05%; ISO 527-3 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |
|||
Secant Modulus, TD | 0.703 GPa | 102 ksi | ASTM D 882 A |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Secant Modulus, TD | 0.700 GPa | 102 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TN2005 EVA General Film Copolymer TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e.. |