Polymer Property : Secant Modulus, TD = 2.00 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 2.00 GPa
290 ksi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc..
Secant Modulus, TD 2.00 GPa
290 ksi
ASTM D882
Solvay Specialty Polymers Ajediumâ„¢ KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu..