Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
NOVA Chemicals Novapol® TD-9022-C Superhexene LLDPE
Puncture value is 60 J/mm. Additive Package: Antiblock.Applications: industrial liners, heavy duty packaging.Film properties are typical of 25 µm blown film extruded at a blow-up ratio of 2.5:1, b..
Secant Modulus, TD 0.190 GPa
27.6 ksi
at 1%; ASTM D882
NOVA Chemicals Novapol® TD-9022-D Super Hexene Film Resin
Excellent dart impact, High strength, High toughnessApplications: Retail trash bagsAdditives: Process stabilizer, Slip/antiblockFilm properties are typical of blown film extruded at a blowup ratio o..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin
Film Properties. Features: Exceptional toughness, high strength with thin films.Applications: Thin films, premium trash bags, ice bags.Data provided by the manufacturer.
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin
Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer.
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin  (discontinued **)
Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Huntsman PE1205 EVA Film Extrusion  (discontinued **)
2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging ..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film
Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ LD1905F Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE, LLDPEContains 1500 ppm slip agent and 2600 ppm antiblocking agentRecommended Applications:General purpose bagVeg..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
SCG Chemicals EL-Leneâ„¢ LD1905FA Low Density Polyethylene Film
Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR..
Secant Modulus, TD 0.190 GPa
27.6 ksi
1%, Flexural; ASTM D882
Braskem Flexus® 7200 LLDPE Cast Film Extrusion
Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Huntsman PE1203 EVA Film Extrusion  (discontinued **)
2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging ..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin  (discontinued **)
Film Properties. Features: High strength and toughness, low gel count, intended for narrow die gaps.Applications: Stretch wrap, blend resin.Data provided by the manufacturer.
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Copyright © lookpolymers.com All Rights Reserved