Polymer Property : Secant Modulus, MD = 58.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.400 GPa
58.0 ksi
ISO 527-3
Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film
Borclear RD738CF is a slip and antiblock formulation propylene alpha olefin copolymer resin. It is suitable for the manufacturing of unoriented film on chill roll process.Borclear RD738CF is suitabl..
Secant Modulus, MD 0.400 GPa
58.0 ksi
ISO 527-3
Borealis Borclear™ RE718CF Propylene Alpha Olefin Copolymer for Metallizable Cast Film
Borclear RE718CF is a propylene alpha olefin copolymer resin formulation with antiblocking agent and without Ca-stearate, especially developed for the manufacturing of unoriented cast films for meta..
Secant Modulus, MD 0.400 GPa
58.0 ksi
ASTM D882
NOVA Chemicals Sclair® 14J1 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, high strength and toughness.Applications: Produce film.Data provided by the manufacturer.
Secant Modulus, MD 0.400 - 2.90 GPa
58.0 - 420 ksi
Average value: 1.69 GPa Grade Count:25
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..