Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | 0.01; ASTM D882 |
Eastman 1925F Polyethylene Film
(discontinued **) Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good.. |
|||
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | 1% Secant; ASTM D882 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | 1% Secant; ASTM D882 |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | 0.01; ASTM D882 |
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
(discontinued **) Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced.. |
|||
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | 1% Secant; ASTM D882 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | 1% Secant; ASTM D882 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Secant Modulus, MD | 0.186 GPa | 27.0 ksi | ASTM D882 |
Huntsman PE8010 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |