Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
M. Holland Company LD120 LDPE
(discontinued **) Features: Good Processability, Medium Strength, Good ToughnessUses: Industrial Applications, Liners, Packaging, Shrink WrapProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Secant Modulus, MD | 0.179 - 1.05 GPa | 26.0 - 152 ksi | Average value: 0.427 GPa Grade Count:13 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 16501F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 16501F6 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets .. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 16501F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Secant Modulus, MD | 0.179 GPa | 26.0 ksi | ASTM D882 |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Secant Modulus, MD | 0.179 - 0.207 GPa | 26.0 - 30.0 ksi | Average value: 0.201 GPa Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |