Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 2.413 - 3.916 GPa | 350.0 - 568.0 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh.. |