Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.840 GPa | 122 ksi | ASTM D882 |
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |