Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.350 GPa | 50.8 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu.. |
|||
Secant Modulus, MD | 0.350 GPa | 50.8 ksi | ISO 527-3 |
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi.. |