Polymer Property : Shear Strength = 3000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
ND Industries 530 Shaft & Bearing Retainer Retaining Compound
General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec ..
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
ND Industries 560 Shaft & Bearing Retainer Retaining Compound
High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
ND Industries 567 Shaft & Bearing Retainer Retaining Compound
High temperature retainer for engine cylinder liners and heat exchanger tubes
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
ND Industries SuperGlue Ethyl 300
General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
ND Industries SuperGlue Ethyl 395
General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste
BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid
Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid
Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste
Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste
Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond ..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste
SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common..
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Lap; ASTM D1002
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste
BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste
Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid
Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste
SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra..
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Lap; ASTM D1002
3M Scotch-Weld™ RT09 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..
Shear Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Lap; ASTM D1002
3M Scotch-Weld™ RT20 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..
Shear Strength 17.2 - 20.7 MPa
2500 - 3000 psi
Adhesive
Abatron Metalfix-L™ Aluminum-Filled, Structural Adhesive Putty; Liquid
Metalfix-L™ is a fluid-pourable version of MetalFix-P™. For patterns, molds, prototypes, casting, and all applications where a castable, fluid, MetalFix-P™ is needed. Excellent for tooling. Techn..