Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 62.1 - 68.9 MPa | 9000 - 10000 psi | Average value: 63.4 MPa Grade Count:6 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Shear Strength | 56.0 - 69.0 MPa | 8120 - 10000 psi | Average value: 63.0 MPa Grade Count:6 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Shear Strength | 55.2 - 68.9 MPa | 8000 - 10000 psi | Die; Bare Si die on alumina |
Lord Adhesives 6100 Silver Conductor LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di.. |