Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6401 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6403 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6404 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6405 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6502 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6503 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6402 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | |
Resinlab® CYNERGY CA6501 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | Overlap, Abraded Aluminum, Cohesive Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | Overlap, 14 days, Cohesive Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | Overlap, 20% Bleach for 14 days, Cohesive Failure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 25.9 MPa | 3750 psi | Overlap, 14 days, Cohesive Failure |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |