Mechanical Properties Metric English Comments
Shear Strength 1.60 MPa
232 psi
Sawbones Solid Rigid Polyurethane Foam 10 pcf Density
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech..
Shear Strength >= 1.60 MPa
>= 232 psi
ISO 1922
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..
Shear Strength >= 1.60 MPa
>= 232 psi
ISO 1922
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..