Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 97.0 MPa | 14100 psi | Estimated from similar grades.; ASTM D732 |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Shear Strength | 97.0 MPa | 14100 psi | ASTM D732 |
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. E.. |
|||
Shear Strength | 97.0 MPa | 14100 psi | ASTM D732 |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Shear Strength | 97.0 MPa | 14100 psi | ASTM D732 |
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2) A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, .. |
|||
Shear Strength | 97.0 MPa | 14100 psi | ASTM D732 |
Haysite HST-II Glass Reinforced Polyester Sheet, Electrical Grade UL, Inc. has granted HST-II the highest thermal recognition ever achieved by any glass polyester laminate (U.L. File No. E81893). HST-II has a 220º C/210º C rating for 1/8" thick and heavier,.. |
|||
Shear Strength | 97.0 MPa | 14100 psi | ASTM D732 |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
Shear Strength | 97.0 MPa | 14100 psi | |
Specialty Materials 5521 Boron Epoxy Prepreg Tape Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,.. |
|||
Shear Strength | 97.2 MPa | 14100 psi | Ultimate; ASTM D3846 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
Shear Strength | 97.2 MPa | 14100 psi | Ultimate; ASTM D3846 |
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle.. |
|||
Shear Strength | 97.2 MPa @Temperature 22.8 °C |
14100 psi @Temperature 73.0 °F |
Ultimate; ASTM D3846 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |