Mechanical Properties Metric English Comments
Shear Strength 91.0 MPa

@Temperature 23.9 °C
13200 psi

@Temperature 75.0 °F
In-Plane, Dry, 365° Autoclave Cured; ASTM D3518
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, IM7 Unitape Reinforced
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois..
Shear Strength 91.0 MPa
13200 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
Shear Strength 91.0 MPa
13200 psi
ASTM D732
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Shear Strength 91.0 MPa
13200 psi
ASTM D732
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)