Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.880 MPa | 1288 psi | Lap |
Epoxy Technology EPO-TEK® H27D Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H27D is a two component, silver-filled epoxy adhesive designed for semiconductor and hybrid-microelectronic packaging applications.Advantages & Application Notes: Rheo.. |