Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 84.1 MPa | 12200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Shear Strength | 84.1 MPa | 12200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Shear Strength | 84.1 MPa @Thickness 15.7 mm |
12200 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Shear Strength | 84.1 MPa | 12200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Shear Strength | 84.1 MPa | 12200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Shear Strength | 84.1 MPa | 12200 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Shear Strength | 84.1 MPa | 12200 psi | Short Beam |
Hexcel® HexPly® EH04 Epoxy Resin System, M35J Fiber MS35J 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |
|||
Shear Strength | 84.1 MPa | 12200 psi | Short Beam |
Hexcel® HexPly® EH04 Epoxy Resin System, MS40 Fiber MS40 120 24" EF04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |
|||
Shear Strength | 84.1 MPa | 12200 psi | Short Beam |
Hexcel® HexPly® EH04 Epoxy Resin System, AS4C Fiber AS4C 150 24" EH04 35%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |