Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 38.6106 - 78.5 MPa @Temperature 150 - 360 °C |
5600.01 - 11400 psi @Temperature 302 - 680 °F |
Average value: 61.7 MPa Grade Count:6 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Shear Strength | 78.5 - 78.5 MPa @Temperature 150 - 150 °C |
11400 - 11400 psi @Temperature 302 - 302 °F |
Average value: 78.5 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyimide, Unfilled |