Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 50.0 - 76.5 MPa | 7250 - 11100 psi | Average value: 61.7 MPa Grade Count:5 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |