Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
ND Industries 530 Shaft & Bearing Retainer Retaining Compound General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec .. |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
ND Industries 560 Shaft & Bearing Retainer Retaining Compound High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
ND Industries 567 Shaft & Bearing Retainer Retaining Compound High temperature retainer for engine cylinder liners and heat exchanger tubes |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
ND Industries SuperGlue Ethyl 300 General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
ND Industries SuperGlue Ethyl 395 General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-L™ Steel-Filled, Structural Adhesive Putty; Liquid Ferrobond-L™ is a fluid pourable Ferrobond-P™. Casting version of Ferrobond-P™. Choose when flowing consistency is needed for pouring. Excellent for tooling. Technical Characteristics: A: 23 lbs.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond .. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste Ferrobond-P™ is a steel-filled, structural adhesive putty. Repair or fill metal components, castings, tanks, and magnetic fixtures. Preferred to Metalfix-P™ where heavier weight, magnetism, or hig.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra.. |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT09 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT20 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Shear Strength | 17.2 - 20.7 MPa | 2500 - 3000 psi | Adhesive |
Abatron Metalfix-L™ Aluminum-Filled, Structural Adhesive Putty; Liquid Metalfix-L™ is a fluid-pourable version of MetalFix-P™. For patterns, molds, prototypes, casting, and all applications where a castable, fluid, MetalFix-P™ is needed. Excellent for tooling. Techn.. |