Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.03 - 1.38 MPa | 150 - 200 psi | Tensile, Al to Al |
Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of .. |
|||
Shear Strength | 1.03 - 1.38 MPa | 150 - 200 psi | Tensile, Al to Al |
Master Bond MasterSil 708FR One Part, Flame Resistant Silicone Description: MasterSil 708FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V.1 for thicknesses of .. |
|||
Shear Strength | 0.689 - 1.38 MPa | 100 - 200 psi | Tensile, Al to Al |
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL.. |