Mechanical Properties Metric English Comments
Shear Strength 6.72 MPa
975 psi
Overlap, RT salt water soak for 14 days, Substrate Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 6.72 MPa

@Temperature -29.0 °C
975 psi

@Temperature -20.2 °F
Overlap, HDPE, Adhesive Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 6.72 MPa

@Temperature 82.0 °C
975 psi

@Temperature 180 °F
Overlap, Green FRP, AF/CF
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 6.72 MPa
975 psi
Overlap, NaOH for 14 days, Substrate Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 6.72 MPa
975 psi
Overlap, HCl for 14 days, Substrate Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 6.72 MPa
975 psi
Overlap, Isopropyl Alcohol for 14 days, Substrate Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 6.72 MPa
975 psi
Overlap, Antifreeze Coolant for 14 days, Substrate Failure
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 6.72 MPa
975 psi
Overlap, Etched Aluminum
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 6.72 MPa
975 psi
Overlap, HDPE/HDG, Adhesive Failure
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 6.72 MPa
975 psi
Overlap, 71°C water soak for 14 days, Cohesive Failure
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive