Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 51.7 - 98.0 MPa | 7500 - 14200 psi | Average value: 80.1 MPa Grade Count:8 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Shear Strength | 51.7 MPa @Temperature 22.8 °C |
7500 psi @Temperature 73.0 °F |
Ultimate; ASTM D3846 |
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK) TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al.. |
|||
Shear Strength | 51.7 MPa @Temperature 22.8 °C |
7500 psi @Temperature 73.0 °F |
Ultimate; ASTM D3846 |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |