Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.28 MPa | 475 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 5/32-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 3.28 MPa @Time 1.80e+6 sec |
475 psi @Time 500 hour |
Overlap, Copper, 50% RH, Salt Water Immersion |
3M 4000 UV 5280 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Shear Strength | 3.28 MPa @Time 1.80e+6 sec |
475 psi @Time 500 hour |
Overlap, Copper, 50% RH, Salt Water Immersion |
3M 4000 UV 6580 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Shear Strength | 3.28 MPa @Time 1.80e+6 sec |
475 psi @Time 500 hour |
Overlap, Copper, 50% RH, Salt Water Immersion |
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Shear Strength | 3.28 MPa | 475 psi | Overlap, Nylon 66 |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |
|||
Shear Strength | 3.28 MPa | 475 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 3.28 MPa | 475 psi | Overlap, PTFE, Adhesive Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 3.28 MPa @Temperature 66.0 °C |
475 psi @Temperature 151 °F |
Overlap, Green FRP, AF/CF |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 3.28 MPa | 475 psi | On Douglas Fir |
3M Scotch-Weld™ 3750LM Low Melt Adhesive Excellent "hot tack", fast setting for corrugated, beadboard, repack, recoup and Economical, general purpose and Use with AE II LET applicator onlyInformation provided by 3M |