Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 1/4-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 1.07 MPa | 155 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/8-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 5/32-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 1.07 MPa | 155 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 1.07 MPa | 155 psi | Plate Shear, W Direction |
Hexcel® HexWeb® HRH-36/OX - 3/16 - 3.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 1/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 3/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 1.07 MPa | >= 155 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |