Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.30 g/micron | 33.0 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Dart Drop | 1.30 g/micron | 33.0 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Dart Drop | 1.30 g/micron | 33.0 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips HiD® 9607D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Dart Drop | 1.30 g/micron | 33.0 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Dart Drop | 1.30 g/micron | 33.0 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Dart Drop | 1.30 - 100 g/micron | 33.0 - 2540 g/mil | Average value: 4.92 g/micron Grade Count:158 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |