Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 10.0 g/micron | 254 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® HD 5301 FB HDPE Film Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi.. |
|||
Dart Drop | 10.0 g/micron | 254 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |