Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 66.9 g/micron | 1700 g/mil | ASTM-D1709A |
Westlake Mxsten CV77515 Polyethylene Plastomer Mxsten CV Plastomer CV77515 resin is a polyethylene plastomer designed for blown film extrusion and food packaging that contains 1,000 ppm slip and no antiblock additives. Films produced with this r.. |
|||
Dart Drop | 66.9 g/micron | 1700 g/mil | ASTM D1709A |
Westlake Mxsten CV77516 Polyethylene Plastomer Mxsten CV Plastomer CV77516 resin is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a very low se.. |