Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 8.90 g/micron | 226 g/mil | ASTM D1709 |
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film ( |