Polymer Property : Dart Drop = 30.26 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 30.26 g/micron
768.6 g/mil
ASTM-D1709
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve..