Mechanical Properties Metric English Comments
Dart Drop 11.4 g/micron
290 g/mil
ASTM-D1709
Westlake EB502 12.5% EVA Copolymer
Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea..
Dart Drop 11.4 g/micron
290 g/mil
ASTM D1709
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
Dart Drop 11.4 g/micron
290 g/mil
ASTM D1709
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr..