Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 10.0 g/micron
254 g/mil
Calculated from thickness
SIDPEC EGYPTENE® HD 5301 FB HDPE Film
Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi..
Dart Drop 10.0 g/micron
254 g/mil
Calculated from thickness
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film
Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch..