Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil LD 071.MU Blown Film Resin
(discontinued **) LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through .. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through .. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ISO 6383/2 |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil LD 316.19 High Clarity, High Impact Film Resin LD 316.19 has improved impact strength and heat sealability versus homopolymer clarity film resins. Applications include frozen and other food packaging, as well as profile extrusion.Information pr.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil LDPE LD 368HD Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Elmendorf Tear Strength TD | 150 g | 150 g | ASTM D1922 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |