Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 538 - 627 MPa
78000 - 91000 psi
Eagle Brass 18665 MSP1, Extra Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Tensile Strength, Ultimate 524 - 627 MPa
76000 - 91000 psi
Eagle Brass 510 Phosphor Bronzes 5% A, Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Ultimate 538 - 627 MPa
78000 - 91000 psi
Eagle Brass 752 Nickel Silver 18%, Hard
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Tensile Strength, Ultimate 517 - 627 MPa
75000 - 91000 psi
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..