Tensile Strength, Ultimate 430 - 550 MPa
62400 - 79800 psi
SSAB Tunnplat Domex® 355MC HSLA Steel
HSLA SteelCharacteristics: For hot-dip galvanizing, a thin Zn coating (50-80 microns) is specified.Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better pr..
Tensile Strength, Ultimate 480 - 550 MPa
69600 - 79800 psi
Wire
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Drawn Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate 450 - 550 MPa
65300 - 79800 psi
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Rolled Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate 500 - 550 MPa
72500 - 79800 psi
Rod
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Drawn Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate 450 - 550 MPa
65300 - 79800 psi
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Rolled Copper Alloy
Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un..
Tensile Strength, Ultimate 500 - 550 MPa
72500 - 79800 psi
Rod
CLAL-MSX ARCAP Anticorrosion AP1C H12 1/2 hard, Drawn Copper Alloy
Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un..
Tensile Strength, Ultimate 500 - 550 MPa
72500 - 79800 psi
Rod
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 20-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 25-16 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 27-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 30-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 48.0 - 550 MPa
6960 - 79800 psi
Average value: 180 MPa Grade Count:56
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Copyright © lookpolymers.com All Rights Reserved