Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 14.0 - 26.0 MPa | 2030 - 3770 psi | Average value: 18.9 MPa Grade Count:11 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 1.59 - 26.0 MPa | 231 - 3770 psi | Average value: 9.34 MPa Grade Count:33 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |