Tensile Strength, Ultimate 50.0 - 228 MPa
7250 - 33000 psi
Average value: 68.5 MPa Grade Count:33
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Ultimate 45.0 - 228 MPa
6530 - 33000 psi
Average value: 65.6 MPa Grade Count:156
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 62.1 - 228 MPa
9000 - 33000 psi
Average value: 161 MPa Grade Count:37
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..