Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 50.0 - 205 MPa @Temperature -50.0 - 250 °C |
7250 - 29700 psi @Temperature -58.0 - 482 °F |
Average value: 124 MPa Grade Count:1 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 110 - 205 MPa | 16000 - 29700 psi | Average value: 159 MPa Grade Count:7 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |