Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1200 - 1400 MPa
174000 - 203000 psi
MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
Cast, reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Tensile Strength, Ultimate 1200 - 1400 MPa
174000 - 203000 psi
SSAB Tunnplat Docol® 1200 DP High-strength Steel
The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel ..
Tensile Strength, Ultimate 1200 - 1400 MPa
174000 - 203000 psi
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me..
Tensile Strength, Ultimate 1390 - 1400 MPa
202000 - 203000 psi
Latrobe Lescalloy® UT-18 VAC-ARC ; 1.25 in. round High Strength Alloy Steel
UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting i..