Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1170 - 1310 MPa | 170000 - 190000 psi | Solution Annealed & Aged |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |
|||
Tensile Strength, Ultimate | 1070 - 1310 MPa | 155000 - 190000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way).. |
|||
Tensile Strength, Ultimate | 1030 - 1310 MPa | 150000 - 190000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Tensile Strength, Ultimate | 1100 - 1310 MPa | 160000 - 190000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or.. |
|||
Tensile Strength, Ultimate | 1100 - 1310 MPa | 160000 - 190000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Tensile Strength, Ultimate | 1070 - 1310 MPa | 155000 - 190000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al.. |