Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 621 - 689 MPa
90000 - 100000 psi
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr..
Tensile Strength, Ultimate 414 - 689 MPa
60000 - 100000 psi
Meehanite CHS Corrosion Resisting Cast Iron
Type CHS is a higher strength material with good shock resistance. Compositional adjustments are made to suit exact service requirements. Recommended for use for components subjected to concentrat..
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Meehanite Ductliron® SP-80 Nodular Graphite Ductile Iron
Type SP-80 possesses in the as-cast condition more than twice the strength of conventional gray cast iron in combination with exceptional toughness. It has a predominantly pearlitic structure, is r..
Tensile Strength, Ultimate 414 - 689 MPa
60000 - 100000 psi
Meehanite HS Heat Resisting Cast Iron
Type HS compares very favorably from a strength standpoint with any heat resisting metal. Compositional adjustments are made to suit the exact service conditions. It machines easily and provides m..
Tensile Strength, Ultimate 586 - 689 MPa
85000 - 100000 psi
Annealed temper
Special Metals INCONEL® 601GC® Nickel Superalloy
Data provided by the manufacturer, Special Metals.
Tensile Strength, Ultimate 627 - 689 MPa
91000 - 100000 psi
Eagle Brass 260 Cartridge Brass, Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Ultimate 586 - 689 MPa
85000 - 100000 psi
Eagle Brass 521 Phosphor Bronzes 8% C, Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Eagle Brass 7026 Copper Nickel, Annealed
7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company
Tensile Strength, Ultimate 552 - 689 MPa
80000 - 100000 psi
Eagle Brass 70265 XP175, Annealed
Information provided by Eagle Brass Company
Tensile Strength, Ultimate 586 - 689 MPa
85000 - 100000 psi
Eagle Brass 725 Copper Nickel Tin, Spring