Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 579 MPa | 84000 psi | |
Kinetics MIM 4605 Low Alloy Steel (As Sintered) Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat .. |
|||
Tensile Strength, Ultimate | 579 MPa | 84000 psi | |
FloMet 316L Stainless Steel FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Ultimate | 579 MPa @Temperature 538 °C |
84000 psi @Temperature 1000 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 579 MPa @Temperature 538 °C |
84000 psi @Temperature 1000 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | >= 579 MPa | >= 84000 psi | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Ultimate | 579 - 648 MPa | 84000 - 94000 psi | |
Eagle Brass 425 Tin Brass 2%, Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Ultimate | 579 - 683 MPa | 84000 - 99000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, Extra Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 579 - 648 MPa | 84000 - 94000 psi | |
Eagle Brass 715 Copper Nickel 30%, Spring 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Ultimate | 579 MPa @Temperature 760 °C |
84000 psi @Temperature 1400 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
Tensile Strength, Ultimate | 579 MPa @Temperature 566 °C |
84000 psi @Temperature 1050 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Ultimate | 579 MPa | 84000 psi | |
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |